This is the walk we take customers through when they visit: the rotomolding floor, the PU foaming line, the fitting benches and the packing area — in the order the product actually moves. These are the machines that run your order.
Everything starts here. LLDPE powder — typically LLD607P or Matrix C6329U for coolers — is weighed per shot, loaded into the mould, and rotated biaxially in the oven until the wall is fully fused. Because the shell comes out in one piece with no seams, the corners and the base are as thick as the walls, which is where a cooler either survives a drop or does not.




Cooling is controlled rather than rushed: a shell that is pulled out hot will warp at the lid seat, and a warped seat is a leaking cooler three months later at your customer's site.
A shell never comes out of the oven perfectly straight, and there is no foam in it yet. Three things happen before foaming: the box is set under a steel plate until the lid seat and the base flatten out; the flash left where the mould halves meet — along the parting line, round the lid slot and the drain boss — is cut away by hand; and the shell then goes to a bench for a second look at those edges before it is released to the foaming queue. Neither step is decoration. Foam poured into a box that is still bowed locks that bow in for good, and an untrimmed edge is what the customer's hands touch every time they open the box.



All of it happens on the shell as it comes off the machine — what reaches the foaming fixtures has already been flattened, trimmed and checked.
Rotomolded shells go straight into our own PU foaming line, where rigid polyurethane is injected between the inner liner and the outer wall. We run the foam at 30 mm on the standard cooler range; the foam we buy is tested at a thermal conductivity of 22.5 mW/(m · K), at least 93% closed cell, which works out to roughly R = 1.33 m²K/W at that thickness.



Foam density and cream time are checked per batch. Under-filled foam shows up as a soft lid and a short ice-retention time, so this is one of the few steps where we slow production down on purpose.
On a cooler, the parts that fail first are rarely the shell — it is the latch, the gasket and the drain plug. Ours are assembled and checked on benches by the same team that packs them: silicone gasket seated evenly in the channel, latch tension set so the lid closes with one hand, drain plug tested for leakage before the unit leaves the bench.



Component materials are documented on our certifications page, including the FDA and LFGB reports for the gasket and latch, RoHS for the lid pin, and the GB 4806.9 report for the drain fitting.






Third-party inspection is welcome — SGS, BV or your own QC team can be booked on the day of loading.
On moulds: the aluminium moulds are machined in an affiliated mould shop next door, and we also accept rotational mould orders when a customer needs a new shape. Mould design is handled by the engineering team, not on this production floor.
Plan for about half a day. We usually start in the sample room so you can put your hands on the products first, then walk the floor in production order — rotomolding, flattening and trimming, foaming, assembly, packing — and finish at a table with the drawings and the quotation.



Tap any photo to open it larger.
On the floor you can also compare surface finishes (matt, camo, marble effect), handle the accessory set (divider board, basket, EVA pad, wheel kit, drain valve) and review logo placement on a real unit rather than a rendering. If you cannot travel, we photograph or video the exact unit we would ship to you and send colour chips by courier.
We are in Ningbo, Zhejiang, under an hour from Ningbo Lishe International Airport and about two hours from Shanghai by high-speed rail. Send us your dates and we will confirm the schedule, the address and who will meet you.